Effects of the Pressure-Holding Time on the Electrochemical Properties of Mm_(0.3)Ml_(0.7)Ni_(3.55)Co_(0.75)Mn_(0.4)Al_(0.3) Metal Hydride Electrodes

Tian Xiao1,Liu Xiangdong2,Yao Zhanquan 2,3,Hai Shan 1(1.Inner Mongolia Key Laboratory for Physics and Chemistry of Functional Materials,Inner Mongolia Normal University,Huhhot 010022,China)(2.Inner Mongolia University of Technology,Huhhot 010051,China)(3.Inner Mongolia Agricultural University,Huhhot 010018,China)  
The Mm0.3Ml0.7Ni3.55Co0.75Mn0.4Al0.3 metal hydride electrodes were prepared at pressure-holding time of t(t=10,15,20 and 25 min).The effects of the pressure-holding time on the activation performance,maximum discharge capacity,discharge potential characteristic and cycle stability of the electrode were investigated.The mechanism of the effect of the pressure-holding time on the electrochemical properties of metal hydride electrodes was also discussed in detail.The results show that the pressure-holding time has no effect on the activation performance of the electrode basically,and the other electrochemical properties of the electrodes are improved firstly and then degenerated with increasing of pressure-holding time.The electrode at pressure-holding time of 15 min exhibits the best electrochemical properties.The improvements of the electrochemical properties are attributed to the increase of the charge-transfer reaction rate on the alloy and the decrease of the internal resistance of the electrodes.
Download(CAJ format) Download(PDF format)
CAJViewer7.0 supports all the CNKI file formats; AdobeReader only supports the PDF format.
©CNKI All Rights Reserved