Corrosion Behavior of X65 Steel in CO_2 Acidic Solution at Different Temperature

LIU Yong-dan1,2,LIU Hai-lang2,WANG Bao-jian2(1.Lanzhou University of Technology,Lanzhou 730050,China;2.Jiangxi University of Science and Technology,Ganzhou 341000,China)  
X65 steel specimens were tested in an acidic solution containing CO2 with a pressure of 1 MPa at 60-150 ℃ for 72 h in an autoclave.XRD,EPMA,SEM and weight-loss methods were used to analyze the corrosion products and corrosion rates.The results showed that the corrosion rates at 60 ℃,90 ℃,120 ℃ and 150 ℃ were 10.97,3.70,8.37 and 18.97 mm·a-1 respectively.Protective films of FeCO3 were not generated at 60 ℃ resulting in serious corrosion.Fine and compact protective films of FeCO3 were formed at 90 ℃ and reduced the corrosion rate markedly.The FeCO3 films were relatively fine but scattered at 120 ℃ and were coarse and loose at 150 ℃ and thus increased the corrosion rate.
【CateGory Index】: TG142.41
Download(CAJ format) Download(PDF format)
CAJViewer7.0 supports all the CNKI file formats; AdobeReader only supports the PDF format.
【Citations】
Chinese Journal Full-text Database 1 Hits
1 Zheng Jiashen (Central China University of Science and Technology);The Research Situation about CO_2 Corrosion[J];Fault-block Oil & Gas Field;1996-01
【Co-citations】
Chinese Journal Full-text Database 10 Hits
1 CHEN Mei-bao JIANG Yu-rong(Chongqing University of Science and Technology,Chongqing 400042);Analysis of the Fatigue Crack Fractograph of X60 Pipeline Steel after Per-tension Deformation[J];;2005-04
2 ZHANG Guoan LU Minxu WU Yinshun (Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083);Morphology and microstructure of CO_2 corrosion scales[J];Chinese Journal of Materials Research;2005-05
3 LI Jin-bo,ZUO Jian-eDepartment of Environmental Science and Engineering,Tsinghua University,Beijing 100084;INFIUENCE OF TEMPERATURE AND SULFUR ION ON CARBON DIOXIDE CORROSION BEHAVIOR OF N80 STEEL[J];Corrosion Science and Protection Technology;2009-01
4 ZHAO Xue-fen,YAO An-lin,ZHAO Zhong-gang(Southwest Petroleum Institute,Chengdu 610500,China);THE ANALYTIC HIERARCHY PROCESS OF INFLUENCING FACTORS IN CARBON DIOXIDE CORROSION[J];Corrosion & Protection;2006-04
5 WEI Ai-jun1,HUO Fu-yong1,CHENG Shi-bao2,DANG Xiao-li2,(1.Xi′an Shiyou University,Xi′an 710065,China;2.SINOPEC Pipeline Storage & Transportation;Xuzhou;3.PetroChina Liaohe Oilfield Company Shenyang oil Production Plant Shengyang,China);Simulating Study of the Influence of CO_2 on Corrosion in Oil pipelines[J];Corrosion & Protection;2008-07
6 CHEN Li~1 LIU Wei~2 LI Zhong~3 DAI Cai-li~2 (1.Linpan Oil Production Company of Shengli Oilfield,Dongying 257061,China; 2.China University of Petroleum,Dongying 257061,China 3.Gudao Oil Production Company of Shengli Oilfield,Dongying 257061,China);Selection and Evaluation of Corrosion Inhibitors Used for Oil Wells in Linpan Oilfield[J];Corrosion & Protection;2008-12
7 ZHOU Qi 1, JI Gen shun 2, YANG Rui cheng 1, XU Jian lin 1, ZHANG Wang feng 2 (1. College of Materials Science and Engineering, Gansu Univ. of Tech., Lanzhou 730050, China; 2. Xi'an Jiaotong Univ., Xi'an 710049, China );Banded structure and hydrogen-induced cracking in pipe-l ines steel[J];Journal of Gansu University of Technology;2002-02
8 Zhu Tao1,2,Jiang Haitao3,Xu Hongxun3,Tian Zhiqiang3,Li Zhongyi2(1.Central Iron & Steel Research Institute,Beijing 100081,China;2.Ma'anshan Iron & Steel Co.,Ltd.,Ma'anshan 243000,Anhui,China;3.School of Materials Science and Engineering,University of Science and Technology Beijing,Beijing 100083,China);Process,Microstructure and Properties of Thick X80 Pipeline Steel Produced by Hot Continuous Rolling[J];Iron Steel Vanadium Titanium;2009-02
9 Luo Yi (Huazhong University of Science and Technology) Luo Lin (Central South Institute of Architecture Design);ANALYSIS OF FAILURE OF NATURAL GAS WELL TUBE BY GREY CORRELATION THEORY[J];Reseach On Iron and Steel;2002-03
10 LIU Xing, YANG Wu (Shanghai Research Institute of Materials, Shanghai 200437, China);The Susceptible Environmental Conditions of Stress Corrosion Cracking of Gas Pipelines[J];Materials For Mechanical Engineering;2002-01
©2006 Tsinghua Tongfang Knowledge Network Technology Co., Ltd.(Beijing)(TTKN) All rights reserved