Effects of Wet Drawn Speed on Property of 0.92wt.%C Brass-Plated Steel Wire Used for Steel Cord

LIU Shi-jun;QIAN Qing-sheng;ZHANG Zheng-yu;MEI Yi-dong;WANG Jian;Technology Center of Jiangsu Xingda Steel Tyre Cord Co.,Ltd.;  
The 0.92 wt.%C brass-plated steel wire with diameter of 1.80 mm was drawn at different drawing speeds under the same wet drawing conditions.The properties of the obtained filaments with diameter of 0.3 mm were studied by torsion delamination test and Hunter-type fatigue test.The results showed that filament delamination occurred when the wet drawing speed exceeded 13m·s-1.With the increase of wet drawn speed,the torsion value and Hunter-type fatigue limit dropped.The temperature of steel wire rose as the wet drawing speed increased,resulting in cementite dissolution,which is the main reason for property degradation of the filament.
【CateGory Index】: TG356;TG142
Download(CAJ format) Download(PDF format)
CAJViewer7.0 supports all the CNKI file formats; AdobeReader only supports the PDF format.
【Citations】
Chinese Journal Full-text Database 5 Hits
1 DONG Yan,FANG Feng,JIANG Jian-qing,GU Han-yan,TU Yi-you(Southeast University,Nanjing 210096,China);Formation and Deformation of Banded Structure in High Carbon Steel Rod[J];Materials For Mechanical Engineering;2005-08
2 ZHANG Xiao-dan1,GODFREY Andrew1,LIU Wei1,LIU Qing1,2(1.Department of Materials Science and Engineering,Tsinghua University,Beijing 100084,China;2.School of Materials Science and Engineering,Chongqing University,Chongqing 400044,China);Cementite deformation and dissolution in a cold-drawn pearlitic steel wire[J];Heat Treatment of Metals;2009-09
3 HUANG Bao,HE Li-bo,GAO Zhen-feng,XING Na(Technology Center of Angang Steel Company Ltd.,Anshan 114009,China);Production status and development trends of wire rod for steel cord in Asia[J];Metal Products;2011-06
4 Qin Wanxin (Xianpeang Petroleum Steel Tube and Wire Rob Plant);Drawing Steel Wires at High Speed[J];STEEL WIRE PRODUCTS;1995-06
5 Qian Qingsheng;Wang Xiuli;Liu Shijun;Yao Lili;Ni Zifei;Miao Weigang;Jiangsu Xingda Steel Tyre Cord Co.,Ltd.;;Microstructure and mechanical properties of C92D2 steel wire rod for steel cord[J];Heat Treatment of Metals;2013-11
【Co-citations】
Chinese Journal Full-text Database 10 Hits
1 Zhang Pengyuan,Sui Xiaohong,Su Hongying,Xie Guangqun,Ma Huixia(Technology Center of Angang Steel Co.,Ltd.,Anshan 114009,Liaoning,China);Banded Structure in Mn-bearing Structural Steel and Its Influence on Mechanical Properties[J];Angang Technology;2010-05
2 LIU Ga,WANG Bo-jian WANG Ping-huai,SHI Xiao-li(Metallurgy College Xi'an University of Architecture and Technology,Xi'an 710055,China);Research of Quench Process of the Clothing Wire[J];Textile Accessories;2007-06
3 FANG Feng~1,JIANG Jian-qing~1,XU Gui-e~2,LI Zhao-xia~2(1.School of Materials Science and Engineering,Southeast University,Nanjing 210096,Jiangsu,China;2.Department of Engineering Mechanics,Southeast University,Nanjing 210096,Jiangsu,China);Finite Element Analysis of Drawing Process of Wire With Inner Micro-defects[J];Iron & Steel;2006-09
4 YANG Lin-jiang,XIAO Xuan,PENG Tao,YE Li-na,ZHOU Zheng(School of Materials Science and Engineering,Chongqing University,Chongqing 400044,China);Microstructure and Mechanical Properties of Pearlite Steel Wires with Different Strains[J];Materials for Mechanical Engineering;2012-03
5 XIAO Xuan;ZHANG Hang;YANG Lin-jiang;ZHOU Zheng;Materials Science and Engineering College of Chongqing University;;Evolutions of Microstructure and Texture in Direct In-Line Patented High-Carbon Pearlitic Steel Wire during Cold Drawing Process[J];Materials for Mechanical Engineering;2013-10
6 LIN Yijian;Shanghai Open University;;Deformation-induced cementite dissolution under thermal activation[J];Baosteel Technology;2014-01
7 PENG Tao;ZHANG Hang;GAN Wen-ying;ZHOU Zheng;School of Materials Science and Engineering,Chongqing University;;Effects of Rapid Heating Process on Microstructure and Mechanical Properties of Cold Drawn Pearlitic Steel Wires[J];Materials for Mechanical Engineering;2014-01
8 Wan Baoyi;Liu Hongyu;Zhou Peng;Liu Jianhua;Chen Xiaolong;College of Science,Wuhan University of Science and Technology;Hubei Province Key Laboratory of Systems Science in Metallurgical Process;Pangang Group Panzhihua Steel & Vanadium Company Limited;;Changes of Microstructures and Cold Drawing Properties of V-N Microalloyed Tire Cord Steel[J];Iron Steel Vanadium Titanium;2014-02
9 ZHOU Lichu;ZHAO Yufei;HU Xianjun;WANG Lei;LI Fan;FANG Feng;JIANG Jianqing;School of Materials Science and Engineering, Southeast University;Sha-steel Iron and Steel Research Institute of Jiangsu Province;;Effect of Austenitizing on Texture Redistribution of Cold Drawn Pearlitic Steel Wire[J];Chinese Journal of Materials Research;2014-08
10 QIAN Qing-sheng;Technology Center of Jiangsu Xingda Steel Tyre Cord Co., Ltd.;;Study on necking fracture of brass-coated steel wire produced by heat diffusion electroplating during wet drawing[J];Electroplating & Finishing;2015-07
China Proceedings of conference Full-text Database 3 Hits
1 YANG Maolin,ZHAO XiuFang(Shougang Shuicheng Iron & Steel(Group) Co.,Ltd,Liupanshui,553028,Guizhou Province,China);Production Situation and Development Trend of Wire Cord Steel in Home and Abroad[A];[C];2012
2 WANG Bojian, XU Ping, SONG Qinghua, LIU Ga, LIU Shifeng (Metall. Eng. College, Xi’an University of Architecture and Technology, Xi′an 710055, China);Relationship Between Tensile Strength and True Strain of Cold Drawn Pearlitic Steel Wire[A];[C];2008
3 ;Strength scattered errors influence factor of cold drawn carbon steel wire for rope[A];[C];2010
【Secondary Citations】
Chinese Journal Full-text Database 10 Hits
1 Hong Shuli(Strategic Planning Department of Angang Steel Group Co.,Anshan 114021,Liaoning,China);Production Practice of Controlling Lamellar Spacing of Sorbite Structure of Cord Steel Coil[J];Angang Technology;2011-02
2 ZHANG Chi1,WAN Genjie2,SHI Qing3 and CAI Li2(1.Research Institute;2.Tube,Pipe and Bar Business Unit;3.Products & Technique Management Department,Baoshan Iron & Steel Co.,Ltd.,Shanghai 201900,China);Technological Progress in Production of Wire Rods for Tyre Cords by Baosteel[J];Baosteel Technology;2010-01
3 Mi Xiaochuan Chen Jiaguang (Iron & Steel Research Institute);Application of XRD & EBSD in Texture Study of Steel Sheet[J];BAO STEEL TECHNOLOGY;1998-05
4 LIU Ga,WANG Bojian,SHI Xiaoli,BAI He,XU Ping (College of Metallurgical Engineering,Xi'an University of Architecture and Technology,Xi'an 710055);Research Present Situation of Work-hardening and Evolution of Microstructure and Mechanical Properties of Cold Drawing Pearlitic Steel Wires[J];Materials Review;2008-S2
5 HUANG Xiao Xu 1, CAI Da yong 1, YAO Mei 1, LIU Qing 2, N.Hansen 2(1.College of Materials Science & Chemical Engineering, Yanshan University, Qinhuangdao 066004, China; 2.Materials Research Department, Ris National Laboratory, Denmark);Characters of sub structures in plastic deformed metals[J];MATERIAL SCIENCE AND TECHNOLOGY;2000-01
6 WANG Li-zhong~1,WANG Jing-tao~2,HUANG Jun-xia~2,GUO Cheng~1,CHEN Jin-de~1,(1.School of Mechanical Engineering,Xi'an Jiaotong University,Xi'an 710049,China;2.Dept.of Materials Science and Engineering,Nanjing University of Science and Technology,Nanjing 210094,China);Influence of passes during ECAP on spheroidization of cemenite in pearlitic steel[J];Materials Science and Technology;2006-01
7 Jia Husheng; Yang Yanqing; Wu Xiaolei; Kang Mokuang(Northwestern Polytechnical University);Theory of Valence Electron of Bainitic Transformation in Carbon-Depleted Regions of Austenite in Fe-C Alloys[J];MATERIAL SCIENCE AND TECHNOLOGY;1995-04
8 Yandong LIU, Qiwu JIANG, Gang WANG, Yandong WANG, A.Tidu and Liang School of Materials and Metallurgy, Northeastern University, Shenyang 110004, China LETAM-ISGMP UMR CNRS 7078, Ile du Saulcy, 57045, University of Metz, Prance Anshan University of Science and Technology, Anshan 114001, China;Influence of Microstructures and Textures on the Torsional Behavior of Pearlitic Wires[J];材料科学技术(英文版);2005-03
9 Chen Zengtao; Wang Duo(Harbin Polytechnical University);Nucleation Mechanism of Plastic Damage in Metals under High Strain Rate[J];MATERIALS SCIENCE AND ENGINEERING;1995-01
10 HUANG Junxia WANG Jingtao ZHANG Zheng (Technical Center, Baosteel Group Shanghai No1 Iron & Steel Co., Ltd, 200431 Department of Materials Science and Engineering, Nanjing University of Science and Technology, 210094 School of Metallurgical Engineering, Xi'an University of Architecture & Technology, Xi'an 710055);Equal channel angular processing in a pearlitic structured steel[J];Chinese Journal of Materials Research;2005-02
©2006 Tsinghua Tongfang Knowledge Network Technology Co., Ltd.(Beijing)(TTKN) All rights reserved